MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Crucible Steel Aquamet® 18 Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: AQUAMET 18 is an austenitic stainless steel with corrosion resistance comparable to that of Type 304. Its good strength and toughness make it an ideal shafting material for workboats. It provides a stainless alternative to ABS Grade 2 carbon steel shafting, but requires no sleeves nor fiberglass. In certain large diameters, it does offer a strength advantage over AQUAMET 19. It is frequently used on pusher tugs, tow boats, supply boats and fishing trawlers.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  621 MPa
@Thickness 203 - 305 mm
90000 psi
@Thickness 8.00 - 12.0 in
 827 MPa
@Thickness <=44.5 mm
120000 psi
@Thickness <=1.75 in
Tensile Strength, Yield  345 MPa
@Strain 0.2 %,
Thickness 203 - 305 mm
50000 psi
@Strain 0.2 %,
Thickness 8.00 - 12.0 in
Tension
 621 MPa
@Strain 0.2 %,
Thickness <=44.5 mm
90000 psi
@Strain 0.2 %,
Thickness <=1.75 in
Tension
Elongation at Break 35 %35 %in 2"; 8" to 12"
 20 %
@Thickness <=44.5 mm
20 %
@Thickness <=1.75 in
in 2"
Reduction of Area  45 %
@Thickness 203 - 305 mm
45 %
@Thickness 8.00 - 12.0 in
 50 %
@Thickness <=44.5 mm
50 %
@Thickness <=1.75 in
Shear Strength  228 MPa
@Strain 0.2 %,
Thickness 203 - 305 mm
33000 psi
@Strain 0.2 %,
Thickness 8.00 - 12.0 in
 414 MPa
@Strain 0.2 %,
Thickness <=44.5 mm
60000 psi
@Strain 0.2 %,
Thickness <=1.75 in
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 16.5 - 19 %16.5 - 19 %
Iron, Fe >= 62.81 %>= 62.81 %As Remainder
Manganese, Mn 11 - 14 %11 - 14 %
Nickel, Ni 0.50 - 2.5 %0.50 - 2.5 %
Nitrogen, N 0.20 - 0.45 %0.20 - 0.45 %
Phosphorus, P <= 0.060 %<= 0.060 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel 18 Cr-Cb™ Ferritic Stainless steel
304 Stainless Steel
AK Steel 18 SR® Ferritic Stainless steel
303 SE Stainless Steel, cold drawn, bar
304 LN Austenitic Stainless Steel (UNS S30453)

NCRUC029 / 16022

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.