MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow UCON™ 50-HB-260 PAG Lubricant
Categories: Fluid; Lubricant

Material Notes: A water soluble polyalkylene glycol (PAG).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.968 g/cc
@Temperature 100 °C
 1.017 g/cc
@Temperature 40.0 °C
 1.033 g/cc
@Temperature 20.0 °C
Viscosity Measurement 212Index; ASTM D2270, IP 226
 6600@ -18°C, [SUS], Saybolt
Saybolt Viscosity at 100°F 260 SUS
Viscosity Measure 380 cSt
@Temperature 0.000 °C
Saybolt Viscosity at 210°F 63.8 SUS
Kinematic Viscosity at 40°C (104°F) 53 cSt
Kinematic Viscosity at 100°C (212°F) 11.1 cSt
Molecular Weight 970 g/mol
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.000800 µm/m-°C
@Temperature 55.0 °C
Pour Point -40.0 °CASTM D97, IP 15
Flash Point 177 °CPMCC; ASTM D93, IP 34
 238 °CCOC; ASTM D93, IP 36
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4542
 
Descriptive Properties
Weight per Gallon8.62 lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow VORANOL™ RA 800 Polyol
Dow UCON™ 50-HB-100 PAG Lubricant

PDOW2013 / 183660

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.