Pyro-Stack modules comprise strips of high quality spunfibre blanket, compressed and banded with plastic strips and including two stainless steel tubes mounted transversely through the strips remote from the hot face. They can be anchored to the furnace casing in any one of four standard versions, Y, M, T and Eye-bolt.Information provided by Morgan Advanced Materials |