MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Old Hickory Wilco-SLU Kaolin Clay  (discontinued **)
Categories: Ceramic; Clay; Kaolin Clay

Material Notes: Wilco SLU is an aqueous suspension of kaolin produced at 70% solids content. The slurry is deflocculated and rheology stabilized with sodium silicate. The Wilco SLU grade is a highly permeable selection and recognized for its coarse particle size distribution. In a ceramic casting formulation, it offers fast casting rate for reduced casting times and quick firming of the piece upon drainage of the mold and removal of the piece for drying.

Information provided by Old Hickory Clay Company

Key Words: M&M Clays, Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.76 g/cc1.76 g/cc
Bulk Density 1.76 g/cc0.0636 lb/in³
Moisture Absorption <= 30.0 %<= 30.0 %
Particle Size 0.50 µm0.50 µm24.4% of particles less than
 1.0 µm1.0 µm37.4% of particles less than
 2.0 µm2.0 µm49.2% of particles less than
 2.1 µm2.1 µmMedian particle diameter
 5.0 µm5.0 µm71.2% of particles less than
 10 µm10 µm87.4% of particles less than
 <= 20 µm<= 20 µm96.2% of particles less than
pH 5.0 - 7.05.0 - 7.010% solids
Specific Surface Area 10 m²/g10 m²/g
Brookfield Viscosity 250 cP250 cP70% solids dispersed using a Brookfield #3 spindle at 100 rpm
 
Component Elements PropertiesMetricEnglishComments
Al2O3 38.21 %38.21 %
CaO 0.040 %0.040 %
Fe2O3 0.36 %0.36 %
K2O 0.11 %0.11 %
Loss on Ignition(%) 13.51 %13.51 %
MgO 0.020 %0.020 %
Na2O 0.020 %0.020 %
SiO2 45.16 %45.16 %
TiO2 1.77 %1.77 %
 
Descriptive Properties
Casting Rate (Barold)120
CEC/MBI (meg/100 ml)2
Pyrometric Cone Equivalent (PCE)34
Wet Sieve Residue (%)2Wet Sieve Residue, +325 mesh

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
KaMin Polygloss® 90 Kaolin Clay - Ultrafine, high brightness
KaMin Polyfil® WC-426 Kaolin Clay - Calcined
KaMin Polyfil® 70 Kaolin Clay - Calcined
KaMin Lithosperse® 7005CS Kaolin Clay - Surface Treated
KaMin Kamintex® D Kaolin Clay - Calcined, high solids

EOHC924 / 162003

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.