MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lucobit Lucofin® 7440 HFFR EBA MDH Cable Sheathing
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Lucofin® 7410 HFFR is a thermoplastic, halogen free flame retardant and low smoke compound for the insulation and/ or sheathing of cables. This grade is based on ethylene butyl acrylate (EBA) and magnesium di hydrate (MDH). Lucofin® 7410 HFFR combines good extrusion properties with flame retardancy.

The properties of Lucofin® 7410 HFFR are in compliance with VDE 0207 part 24(HM 2/4), VDE 0207 part 23 (HJ2), BS 6724 as well as other power and telecom standards.

Information provided by Lucobit AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.44 g/ccISO 1183
pH 6.0
Mooney Viscosity 40
@Temperature 140 °C
ML (1+4); ASTM D 792
Halogen Content <= 0.050 %IEC 754-1
Melt Flow 6.5 g/10 min
@Load 21.6 kg,
Temperature 150 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 52ISO R 868
Tensile Strength 10.8 MPaAged 7 days @ 110°C; IEC 60811-1-1
 11.5 MPaIEC 60811-1-1
Elongation at Break 120 %Cold; IEC 60811-1-4
 160 %Aged 7 days @ 110°C; IEC 60811-1-1
 185 %IEC 60811-1-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.90e+14 ohm-cmIEC 60167
 2.10e+14 ohm-cm
@Temperature 70.0 °C
7 days water immersion; IEC 60167
Surface Resistance 4.10e+14 ohmIEC 60093
 1.70e+14 ohm
@Temperature 70.0 °C
7 days water immersion; IEC 60093
Dielectric Constant 3.6
@Frequency 50 Hz
IEC 60520
 5.3
@Frequency 50 Hz,
Temperature 20.0 °C
24h water immersion; IEC 60520
Dissipation Factor 0.00735
@Frequency 50 Hz
IEC 60520
 0.0635
@Frequency 50 Hz,
Temperature 20.0 °C
24h water immersion; IEC 60520
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 38 %ISO 4589-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 220 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucobit Lucofin® 7410 HFFR EBA MDH Cable Sheathing
Dow Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer
Dow Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer
Dow Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer
Neutrex Purgex™ 460 Plus Purging Compound

PLUCO953 / 151019

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.