MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hippe PF CP 202 Cellulose Paper Reinforced Phenolic Resin - Sheet
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Cellulose Filled

Material Notes: High voltage applications at power frequencies. High electric strength under oil. Good electrical strength in air under normal humidity.

Information provided by Hippe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 - 1.40 g/ccIEC 1212-2 8.1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 100 MPaIEC 1212-2 5.7
Flexural Strength >= 120 MPaPerpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 7.00 GPaIEC 1212-2 5.2
Compressive Strength >= 300 MPaPerpendicular to laminations; IEC 1212-2 5.3
Shear Strength >= 10.0 MPaParallel to laminations; IEC 1212-2 5.6
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant <= 5.5
@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 60000 V
@Temperature 90.0 °C
Cond., In oil, Parallel to laminations; IEC 1212-2 6.2
Dissipation Factor <= 0.050
@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
Comparative Tracking Index >= 100 VIEC 1212-2 6.4
 
Descriptive Properties
Thermal Endurance120 T.I.IEC 1212-2 7.1
Water Absorption< 550 mgIEC 1212-2 8.2; Test piece 50 x 50 x 10 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cookson Group Plaskon® 440 Mineral Filled Novolac Epoxy Molding Compound
Plenco 2000 Phenolic, Granular, Compression Molded
Kaneka Kane Ace MX-215 Epoxidized Novolac Resin
Hippe PF CP 201 Cellulose Paper Reinforced Phenolic Resin - Sheet
Emerald Performance Materials ERISYS RF50 Resorcinol Modified Phenol Novolac Epoxy Resin

PHIPPE917 / 121921

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.