MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Amco PRIMATOP PP CO 005NB Fractional Melt Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Features:
  • heat aging resistance
  • impact resistance
  • low temperature melt strength
  • good stiffness
Applications:
  • containers
  • pipes
  • toys
  • extrusion coating

Former A-Top Polymers product; part of Amco product line since 2013.

Key Words: FDA 21CFR177.1520
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.902 g/ccmethod B; ASTM D792
Melt Index of Compound 0.45 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 80ASTM D785
Tensile Strength, Yield 4000 psi50 mm/min; ASTM D638
Elongation at Yield 11 %ASTM D638
Flexural Modulus, 1% Secant 160 ksi0.05 in/min; ASTM D790
Izod Impact, Notched NB
@Temperature 22.8 °C
Method A; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 190 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Amco PRIMATOP PP CO 100 NB High Impact Copolymer
Lotte Chemical Titan TITANPRO® SM256 Polypropylene random copolymer
Overview of materials for Polypropylene Copolymer
Ineos N05U-00 Polypropylene Impact Copolymer
Ineos N02G-00 Polypropylene Impact Copolymer

PATOP026 / 79969

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.