MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 2123 Metal Repair Steel/Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: TRA-BOND 2123 is a versatile steel metal/epoxy adhesive formulation developed for modern industrial repair, casting and bonding applications where a steel-like or cast iron finish is required. This easy-to-use adhesive system contains no solvents and cures fairly rapidly at room temperature to a hard, low shrinkage solid, which bonds readily to steel, aluminum, and other metals, wood, concrete, glass, ceramics and many plastics. Fully cured TRA-BOND 2123 is tough and durable, resistant to water, mild acids and alkalis, salts and salt solutions, lubricating oils, petroleum solvents, gasoline, jet fuels, alcohol and many other organic and inorganic materials, While it may be attracted to a magnet, it is essentially an electrical insulator which can be readily drilled, cut, sawed and machined with regular metal working tools Typical repair applications: jigs, molds, dies, fixtures, plumbing, automotive, castings, aircraft, ships, marine, salvage.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.35 g/ccMixed
Solids Content 100 %Reactive Solids Content
Viscosity 32000 cP
@Temperature 25.0 °C
After mixing
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 65
@Frequency 1000 Hz
Dielectric Strength 30.0 V/mil
Dissipation Factor 0.20
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 38.0 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.590 W/m-K
Maximum Service Temperature, Air 135 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg 110 °CUltimate Tg
Shrinkage 0.080 %
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 30 min
 
Descriptive Properties
Color Steel Gray
Mix Ratio, parts by weight100/10Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H61 Thermally Conductive Epoxy
Dow 806A RESIN
Dow 805 RESIN
Devcon Underwater Repair Putty (UW) Epoxy
Cotronics Duralco™ 4461 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant

PTRAC020 / 70948

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.