3M™ Clean-Walk Unframed Mats 5830 Series are a multi-sheeted adhesive system that removes dirt and contaminates from shoe soles, wheels and other passing objects on contact. Comprised of a thin adhesive backed colored base topped by 30 or 0 removable adhesive polyethylene sheets that lock dirt in place until discarded.Information provided by 3M |