MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled; Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength

Processing Method: Injection Molding

Forms: Pellets

Additive: Heat Stabilizer; Lubricant

Information Provided by Teknor Apex

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.010 cm/cm0.0050 - 0.010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 114 MPa16500 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Elongation at Yield 3.0 %3.0 %ASTM D638
Flexural Strength 162 MPa23500 psiASTM D790
Flexural Modulus 4.31 GPa625 ksiASTM D790
Izod Impact, Notched 0.641 J/cm
@Temperature 22.8 °C
1.20 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Strength 11.0 kV/mm
@Thickness 3.00 mm
280 kV/in
@Thickness 0.118 in
ASTM D149
Comparative Tracking Index 500 V500 VUL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.8 µm/m-°C31.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 204 °C400 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 188 °C370 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 0.810 mm
HB
@Thickness 0.0319 in
Oxygen Index 22 %22 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 218 - 235 °C425 - 455 °F
Middle Barrel Temperature 241 - 257 °C465 - 495 °F
Front Barrel Temperature 246 - 268 °C475 - 515 °F
Nozzle Temperature 246 - 268 °C475 - 515 °F
Melt Temperature 216 °C420 °F
 249 - 266 °C480 - 510 °FProcessing Temperature
Mold Temperature 60.0 - 93.3 °C140 - 200 °F
Drying Temperature 79.4 °C175 °F
Moisture Content 0.20 %0.20 %
Injection Pressure 34.5 - 138 MPa5000 - 20000 psi
Screw Speed 60 - 120 rpm60 - 120 rpm
 
Descriptive Properties
AppearanceBlack; Natural Color
Suggested Regrind, max25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill FR® PA6 GF13 FR-N BK 13% Glass Filled
Teknor Apex Chemlon 214 G Nylon 6, 14% Glass Fiber Reinforced
Wellman Wellamid® GF14-60 XE-NBK1 Nylon 6, 14% Glass Fiber Reinforced
Ashley Polymers Ashlene® 630-13G Nylon 6, 13% Glass Reinforced
Ashley Polymers Ashlene® 527LD-14G Nylon 66, 14% Glass Reinforced

PTEKNO409 / 128586

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.