CAS Number: 24937-78-8 FLEXAREN® 14001 – high quality ethylene vinyl acetate copolymer with 14% content of vinyl acetate. Manufactured by high pressure tubular process. FLEXAREN® 14001 is more elastic than LDPE and compatible with a wide range of polymers. It can be processed with the same equipment. Application: - Stretch films
- Agricultural films
- Sealing profiles for windows
- Flexible hoses
Properties: - Flexibility (especially at low temperatures)
- High transparency
- Good mechanical properties
Information provided by Innospec Inc |