MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Chemfab® 500F PTFE Coated Beta Fiberglass Conveyor Belting
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Description: General Notes on Saint Gobain Belting Products:
Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeability for rapid drying, dimensional and thermal stability, and the dynamic strength to stand up to the most rigorous operating conditions. The unique behavior of the materials results in a product that is more practical and cost-effective than conventional belting materials.
Release Properties: The release characteristics of PTFE are superior to those of any other high-temperature material. This non-stick property is retained over a full range of operating temperatures.
Permeability: Our belting combines a maximum amount of open area with good mechanical strength. The result is a very high level of controlled air flow through the belt, maximizing the rate of drying.
Dimensional Stability: The woven reinforcement results in an elongation of approximately 1% under normal mechanical loading, even at temperatures of 550°F. Length distortion is exceptionally low, while width rigidity and stability are enhanced by the high modulus of the reinforcement.
Thermal Stability: Chemfab® brand belting may be used continuously at temperatures up to 550°F without reducing its performance.
Dynamic Stability: Our belting has been subjected to static and dynamic tests which indicate that it can withstand all normal operating conditions affecting service life.
Chemical Resistance: PTFE surfaces are unaffected by most chemicals and solvents.

Notes on 500F PTFE Coated Beta Fiberglass Conveyor Belting:
Chemfab® 500F utilizes a tightly woven Beta® fiberglass substrate, lightly coated with PTFE. Its primary use is for aerospace applications (e.g., space shuttle, international space station). For applications that require electrical static dissipation, Saint-Gobain produces Chemfab® 500GW. This product is silicone free. The substrate is Beta fiberglass and the coating material is PTFE (PTFE = polytetrafluoroethylene). All data based on a 0.008 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 79.17 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break >= 2.0 %Fill/Transverse direction
 >= 6.5 %Warp/Longitudinal direction
Tear Strength Test 7.0Lbs./In. Propagation Tear Strength in fill/transverse direction
 10Lbs./In. for warp/longitudinal Propagation Tear Strength
Tear Strength 90.0 pliTensile Strength (Fill)
 95.0 pliTensile Strength (Warp)
Taber Abrasion, mg/1000 Cycles >= 750
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 550 °F
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) >= 0.80
 
Descriptive Properties
Weight (oz/yd^2)7.6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Chemfab® 1584G PTFE Coated Fiberglass Conveyor Belting
Saint-Gobain Chemfab® 1565V PTFE Coated Fiberglass Conveyor Belting
Saint-Gobain Chemfab® 1584N PTFE Coated Fiberglass Conveyor Belting
Overview of materials for Styrenic Elastomer (TES)
Saint-Gobain Chemfab® 1589 PTFE Coated Fiberglass Conveyor Belting

CSTGQZ112 / 2241

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.