MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound OF008A Polyphenylene Sulfide, Branched (PPS, Branched) (Asia)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: LNP THERMOCOMP OF008A compound is based on branched Polyphenylene Sulfide (PPS) resin containing 40% glass fiber.

Features: High Stiffness,Structural

Information provided by SABIC

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 160 MPa5 mm/min; ISO 527
 178 MPa5 mm/min; ASTM D638
Elongation at Break 1.2 %5 mm/min; ISO 527
 1.7 %5 mm/min; ASTM D638
Flexural Strength 190 MPayield, 2 mm/min; ISO 178
 248 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 13400 MPa2 mm/min; ISO 178
 14260 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 101 JASTM D256
Izod Impact, Unnotched 587 J/mASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 21.0 kJ/m²80*10*4; ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index 250 - 400 VUL 746A
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness >=1.50 mm
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
UL 746A
 >= 120 sec
@Thickness >=6.00 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 26.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 272 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 261 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 220 °CUL 746B
UL RTI, Mechanical with Impact 200 °CUL 746B
UL RTI, Mechanical without Impact 220 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.450 mm
UL 94
 5VA
@Thickness >=3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 320 - 330 °C
Zone 3 330 - 345 °C
Melt Temperature 315 - 320 °CInjection Molding
Mold Temperature 140 - 165 °C
Drying Temperature 120 - 150 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81755 / 289702

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.