MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celstran® POM-GF35-04 AF3001 POM, 35% Glass Reinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 30% Glass Fiber Reinforced

Material Notes: Material code according to ISO 1043-1: POM

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 182 MPa50mm/min; ISO 527-2/1A
Elongation at Break 2.05 %5mm/min; ISO 527-2/1A
Tensile Modulus 11990 MPa50mm/min; ISO 527-2/1A
Flexural Strength 285 MPaISO 178
Flexural Modulus 10895 MPaISO 178
Charpy Impact, Notched 41.0 kJ/m²ISO 179/1eA
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 - 110 °Ccavity
 195 - 205 °Chot runner
Feed Temperature 20.0 - 50.0 °C
Zone 1 180 - 195 °C
Zone 2 190 - 200 °C
Zone 3 195 - 205 °C
Zone 4 195 - 205 °C
Die Temperature 195 - 205 °C
Melt Temperature 195 - 205 °C
Drying Temperature 80.0 - 90.0 °C
Dry Time 3.00 hour
Moisture Content <= 0.15 %
Injection Pressure 60.0 - 120 MPa
Hold Pressure 60.0 - 120 MPa
Back Pressure <= 3.00 MPa
Screw Speed 25 rpm
@Diameter 75.0 mm
 35 rpm
@Diameter 55.0 mm
 50 rpm
@Diameter 40.0 mm
 
Descriptive Properties
Injection speedmedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
EN S355K2G3C High Manganese, Structural, Hot Rolled, Quality Steel
Oxford Polymers C-Acetal -30GF-Natural Acetal Copolymer, 30% Glass Fiber Reinforced
KEP Kepital® FG2025 Acetal Copolymer, 25% Glass Fiber
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled

PHCQ195 / 178650

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.