MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade
Categories: Polymer; Thermoplastic; Polymethylpentene (PMP)

Material Notes: TPX® is a 4-methylpentene-1 based polyolefin. TPX is used in a wide variety of applications, including: medical equipment, laboratory ware, small appliances, ovenware, baking cartons, release paper, wire and cable coating, and a number of industrial uses. TPX is manufactured and marketed solely by Mitsui Chemicals, Inc.

Applications:

  • Injection Molded Items:
    • Blood test cells
    • Medical instruments
    • Laboratory ware
    • Coffee maker parts
    • Cosmetic containers
  • Extrusion Molded Items:
    • Sight glass (pipes, sheets)
    • Baking cartons (food containers)
    • Release paper
    • Wire and cable coating
    • Films

Molding Method:

  • Injection
  • Extrusion

Information provided by Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.833 g/ccASTM D1505
Water Absorption 0.010 %24 hours; ASTM D570
Linear Mold Shrinkage 0.021 cm/cmMPC method, MD
Linear Mold Shrinkage, Transverse 0.017 cm/cmMPC method
Melt Flow 26 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 85ASTM D785
Tensile Strength at Break 17.2 MPa5mm/min; ASTM D638
Tensile Strength, Yield 23.0 MPa5mm/min; ASTM D638
Elongation at Break 25 %MPC method, 5mm/min
Modulus of Elasticity 1.28 GPaTangent; ASTM D790
Flexural Strength 35.3 MPa2mm/min; ASTM D790
Flexural Stiffness 140000 psiOlsen Stiffness; ASTM D747
Izod Impact, Unnotched (ISO) 14.7 kJ/m²
@Thickness 2.00 mm,
Temperature 20.0 °C
ASTM D256
Charpy Impact, Notched 0.420 J/cm²
@Thickness 2.00 mm,
Temperature 20.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.12
@Frequency 100 - 1.00e+6 Hz
ASTM D150
Dielectric Strength 65.0 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 117 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Specific Heat Capacity 1.97 J/g-°CASTM C351
Thermal Conductivity 0.000400 cal cm/sec-cm²-°CBS 874A
Melting Point 240 °CMPC Method
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °CASTM D648
Vicat Softening Point 173 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.463n20 D; ASTM D542
Haze 2.0 %ASTM D1746
Transmission, Visible 90 %Mfr. indicates clear but does not quantify
 
Descriptive Properties
AppearanceColorless transparent
Rate of Burning2.54 cm/minASTM D635

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsui TPX® RT18 XB Methylpentene Copolymer
Covestro Makrolon® 2558 Polycarbonate
Mitsui TPX® DX820 Methylpentene Copolymer
Goodfellow TPX® RT31 Injection Molding Grade Polymethylpentene
Mitsui TPX® MX004 Methylpentene Copolymer

PMIT046 / 53227

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.