MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Assab Steels 705M Machinery Steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: ASSAB 705M is an alloyed machinery steel with good hardenability also in heavier sizes. As standard ASSAB 705M is supplied tough hardened with no further heat treatment required. It can be oil hardened to higher mechanical properties if required.

Applications: ASSAB 705M is suitable for induction hardening and can also be nitrided or tuffrided to a surface hardness of 600-650 Vickers.

ASSAB 705M is not suitable for welding but can with certain precautions be repair welded.

AISI /SAE 4340, DIN 34CrNiMo6, W.nr. 1.6582, BS 817M40 (EN 24), AFNOR 35NCD6, JIS SNCM8, SS 2541

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 240700°C tempering temperature. Quenching in oil ø 120. Test piece hardened by oil quenching from 850°C.
 275 - 335Hardness supplied approx.
 320500°C tempering temperature. Quenching in oil ø 120. Test piece hardened by oil quenching from 850°C.
Hardness, Rockwell C 40tempering temperature 500°C. Hardened by oil quenching.
 43 - 5530 mm from the quenched end.
 50tempering temperature 200°C. Hardened by oil quenching.
 49 - 5810 mm from the quenched end.
Tensile Strength at Break 790 MPaRm. 700°C tempering temperature. Quenching in oil ø 120. Test piece hardened by oil quenching from 850°C.
 1100 MPaRm. 500°C tempering temperature. Quenching in oil ø 120. Test piece hardened by oil quenching from 850°C.
Tensile Strength, Ultimate 900 - 1100 MPaRm
Tensile Strength, Yield 690 MPaRe. 700°C tempering temperature. Quenching in oil ø 120. Test piece hardened by oil quenching from 850°C.
 700 MPamin. Re.
 975 MPaRe. 500°C tempering temperature. Quenching in oil ø 120. Test piece hardened by oil quenching from 850°C.
Elongation at Break >= 12 %
 13 %5XD. 500°C tempering temperature. Quenching in oil ø 120. Test piece hardened by oil quenching from 850°C.
 20 %5XD. 700°C tempering temperature. Quenching in oil ø 120. Test piece hardened by oil quenching from 850°C.
Reduction of Area 42.5 %500°C tempering temperature. Quenching in oil ø 120. Test piece hardened by oil quenching from 850°C.
 >= 45 %
 63 %700°C tempering temperature. Quenching in oil ø 120. Test piece hardened by oil quenching from 850°C.
Impact Test >= 20.0 J
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.36 %
Chromium, Cr 1.4 %
Iron, Fe 95.69 %
Manganese, Mn 0.70 %
Molybdenum, Mo 0.20 %
Nickel, Ni 1.4 %
Silicon, Si 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Assab Steels 709M Machinery Steel
AISI 4340 Steel, normalized, 25 mm round
AISI 4340 Steel, annealed, 25 mm round
AISI 1040 Steel, water quenched from 845°C (1550°F), 540°C (1000°F) temper, 100 mm (4 in.) round
AISI 347 Cast Stainless Steel, EN 10088-3

NASSAB18 / 15036

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.