MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Novamid® 3010CF30 BK PA66-CF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Carbon Fiber Filled

Material Notes: 30% Carbon Reinforced

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccdry; ISO 1183
Moisture Absorption 2.00 %Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cmSim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cmSim. To ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 230 MPadry; ISO 527-1/-2
Elongation at Break 2.8 %dry; ISO 527-1/-2
Flexural Strength 343 MPadry; ISO 178
Flexural Modulus 17000 MPadry; ISO 178
Charpy Impact, Notched 10.0 kJ/m²
@Temperature 23.0 °C
dry; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 260 °Cdry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 245 °Cdry; ISO 75-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celstran® PA66-CF20-03 20% Long Carbon Fiber Reinforced Nylon 66
Asahi Kasei Thermylon® N3-25FG-2726 PA66-GF25
Ensinger ENSILON® 6/6 Extruded Nylon 6/6 (PA66)
Envalior Akulon® Diablo HT-HG0 (K-X07029) PA66+PA6-GF50, Dry, 50% Glass Filled, Heat Stabilized
Plastcom SLOVAMID 66 CF 30 TS PA 66 reinforced with 30% carbon fibre, thermal stabilization

PDSM9841 / 161462

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.