MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
OCSiAl TUBALL™ MATRIX 822 Graphene Nanotube Concentrate
Categories: Carbon; Other Engineering Material; Additive/Filler for Polymer

Material Notes: TUBALL™ MATRIX 822 is a versatile conductive additive based on polyol ester carrier to produce masterbatches based on PP, TPU, filled PPS, ABS, PC, PC-ABS, PA, GF PA. Resulting masterbatches can be used for compounding in filled polymers or in combination with other conductive fillers to reduce their content and gain better mechanics/fluidity. TUBALL™ MATRIX 822 is available in pellet form. TUBALL™ is a unique graphene nanotube additive from OCSiAl that provides electrical conductivity at ultralow dosage with minimal impact on the rheological and mechanical properties of the host matrix.

Applications: Extrusion of conductive masterbatches based on thermoplastics, Automotive industry, Other applications where electrical conductivity is required.

Benefits: TUBALL™ MATRIX 822 used as a carrier for master batches, Minimal influence on mechanical properties, Ensures permanent and uniform electrical properties without “hot spots”, Without a significant increase in viscosity or density of the host material.

Information provided by OCSiAl

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.460 g/ccISO 3923-1:2018
Density 1.07 g/ccISO 1183
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 270 °CISO 2592
 
Processing PropertiesOriginal ValueComments
Melt Temperature 40.0 °C10K/min; ISO 11357-1
 
Descriptive Properties
CarrierFatty Acid, Ester of Polyol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EOCSIAL922 / 305661

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.