MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polymer Tailoring PTFA 12 Polypropylene compound
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: PTFA 12 is a tough and rigid halogen-free compound designed for injection moulding engineering components. Initially developed for moulding escalator comb sets, it has since proved beneficial in other electrical components because of its stiffness and durability. It can even replace glass-filled FR nylon compounds in certain applications, due to its thermal and UV-stability ratings and lower specific gravity. Currently available in yellow RAL 1023, other colours and performance permutations can be accommodated. Articles made from this compound will meet the environmental criteria of both the WEEE and ROHS Directives.
  • Polypropylene based
  • Potential replacement for glass-filled nylon compounds
  • Very strong and durable
  • Lower processing temperature(~180ºC) allows for energy savings in production
  • Lower density (specific gravity) means more units per tonne
Currently Available Colours: White, Natural

Information provided by Polymer Tailoring Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 45.0 MPa6530 psiISO 179
Flexural Strength 65.0 MPa9430 psiISO 179
Izod Impact, Notched (ISO) 4.90 kJ/m²2.33 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 112 °C234 °FB120
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 
Descriptive Properties
UV stability>150Kly

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTAIL006 / 297044

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.