MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound KI001XXJ Acetal (POM) Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: LNP LUBRICOMP KI001XXJ compound is based on POM (Acetal) resin containing silicone. Added features of this grade include: Wear Resistant, Healthcare.

Features: Low Extractable,Healthcare,Wear resistant,Food Contact Acceptable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183
Moisture Absorption 0.240 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.024 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.024 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 52.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 55.0 MPa5 mm/min; ASTM D638
Elongation at Break 46 %5 mm/min; ASTM D638
Elongation at Yield 16 %5 mm/min; ASTM D638
Tensile Modulus 2750 MPa50 mm/min; ASTM D638
Flexural Strength 74.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2280 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 81.0 JASTM D256
Izod Impact, Unnotched 1550 J/mASTM D4812
Coefficient of Friction, Dynamic 0.44ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.34ASTM D3702 Modified: Manual
K (wear) Factor 22.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 195 - 205 °C
Zone 3 210 - 220 °C
Melt Temperature 200 - 215 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80839 / 288786

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.