MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company EMI 661 Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D 792
Additive Loading 10 %Primary Additive
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 5800 psiASTM D 638
Elongation at Break 3.0 - 7.0 %ASTM D 638
Tensile Modulus 400 ksiASTM D 638
Flexural Strength 10500 psiASTM D 790
Flexural Modulus 400 ksiASTM D 790
Izod Impact, Notched 1.20 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 5.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.0 ohm-cmASTM D 257
Surface Resistance <= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
Shielding Effectiveness 52 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 54 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 58 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 61 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 64 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 67 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 68 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 72 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 75 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 81 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 84 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 88 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 34.0 µin/in-°FE 831
CTE, linear, Transverse to Flow 63.0 µin/in-°FE 831
 
Processing PropertiesOriginal ValueComments
Melt Temperature 440 - 480 °F
Mold Temperature 150 - 180 °F
Drying Temperature 180 °F
@Time 7200 sec
Moisture Content 0.10 %
Dew Point 0.000 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company EMI 1363 Polyphenylene Sulfide (PPS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 1361 Polyphenylene Sulfide (PPS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 1262 S-80A Ester-based Thermoplastic Polyurethane Elastomer; Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
RTP Company EMI 1063 Polybutylene Terephthalate (PBT); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive
RTP Company EMI 1062 Polybutylene Terephthalate (PBT), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection

PQZTA2904 / 159307

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.