MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Industeel SIRIUS 314 25% Cr - 1.8% Si Heat Resistant Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Description: CLI SIRIUS 314 grade is a fully austenitic stainless steel containing 25% Cr, 20% Ni and 1.8% Si. The alloy is designed for high temperature corrosion resistance applications even in severe conditions. Carbon additions are optimized in order to increase creep properties and mechanical properties. The alloy is well designed for applications up to 1150°C (2102°F) in oxidizing atmospheres, or up to 1050°C (2012°F) in reducing atmospheres. Sulphur, carbon or nitrogen pick up reduce the behavior of the steel. The alloy performs better than Sirius 310 or Sirius 253 grades in most of the applications.

Information provided by manufacturer.

Key Words: EN 10095 X15 Cr Ni Si 25-21 1.4841, AFNOR Z10 CNS 25.20, DIN W. Nr 1. 4841, ASTM Type 314
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 600 MPaTypical after Solution Annealing
Tensile Strength, Yield 285 MPa
@Strain 0.2 %
Typical after Solution Annealing
 305 MPa
@Strain 1 %
Typical after Solution Annealing
Elongation at Break 45 %Typical
Creep Strength 130 MPa
@Temperature 600 °C,
Time 3.60e+6 sec
Modulus of Elasticity 200 GPa
Poissons Ratio 0.333Calculated
Shear Modulus 75.0 GPa
@Temperature 20.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000950 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 - 100 °C
 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
 18.0 µm/m-°C
@Temperature 20.0 - 400 °C
 18.5 µm/m-°C
@Temperature 20.0 - 600 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 25 %
Iron, Fe 53.05 - 53.2 %As remainder
Nickel, Ni 20 %
Silicon, Si 1.8 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum 310Si Austenitic Stainless Steel
Outokumpu 4841 High Temperature Austenitic Stainless Steel
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel
Industeel SIRIUS S12 20% Cr - 1.8% Si Heat Resistant Steel
314 Stainless Steel, Annealed Wire

NINDUST31 / 17569

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.