MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lanxess Addocat® SO PU Catalyst/Activator
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: Product Information: Addocat SO catalyses mainly the crosslinking reaction of the polyol and isocyanate. In the production of polyether and polyester foam Addocat SO is metered separately. As well as having other advantages, this enables equilibrium of the crosslinking and gas formation reactions to be maintained during production. The addition of Addocat SO is normally between 0.03 and 0.5 p.b.w. The accuracy of metering can be improved if Addocat SO is mixed with other components at a ratio suitable to the capacity of the metering pump, e.g. with polymeric plasticizers that do not affect the polyurethane reaction or with polyether polyols based on propyleneoxide, but without ethylene oxide. The mixing ratio applicable to these examples is usually 1 : 4 or 1 : 9.

Function: Catalyst for the production of polyurethanes, e.g. polyether and polyester flexible slabstock foam, hot molded foam, rigid spray foam, 2 C-paints and coatings as well as other polyurethane applications.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 - 1.27 g/cc0.0444 - 0.0459 lb/in³
Viscosity 350 cP350 cP
 
Thermal PropertiesMetricEnglishComments
Melting Point <= -20.0 °C<= -4.00 °FFreezing Point
Boiling Point >= 200 °C>= 392 °F
Flash Point 130 °C266 °FASTM D92, DIN ISO 2592
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.487 - 1.5031.487 - 1.503
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Tin, Sn >= 27 %>= 27 %tin-II
 >= 28 %>= 28 %
 
Descriptive Properties
Appearanceclear, slightly yellowish liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8200 / 208593

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.