MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Pressure Seal 13301 Chlorobutyl
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 13301 is a 30 durometer black colored general purpose Chlorobutyl elastomer. It exhibits good resistance to compression set at moderate temperatures, it will remain non brittle at low temperatures.

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2929
 27
@Temperature 100 °C,
Time 252000 sec
27
@Temperature 212 °F,
Time 70.0 hour
Distilled water aged
 30
@Temperature 70.0 °C,
Time 252000 sec
30
@Temperature 158 °F,
Time 70.0 hour
Heat Aged
 33
@Temperature 100 °C,
Time 252000 sec
33
@Temperature 212 °F,
Time 70.0 hour
Heat Aged
Tensile Strength 1.97 MPa286 psi
 2.469 MPa
@Temperature 70.0 °C,
Time 252000 sec
358.1 psi
@Temperature 158 °F,
Time 70.0 hour
Heat Aged
 2.96 MPa
@Temperature 100 °C,
Time 252000 sec
429 psi
@Temperature 212 °F,
Time 70.0 hour
Heat Aged
Elongation, Ultimate 575 %575 %
 638.25 %
@Temperature 70.0 °C,
Time 252000 sec
638.25 %
@Temperature 158 °F,
Time 70.0 hour
Heat Aged
 649.75 %
@Temperature 100 °C,
Time 252000 sec
649.75 %
@Temperature 212 °F,
Time 70.0 hour
Heat Aged
100% Modulus 0.324 MPa47.0 psi
Tear Strength 5.78 kN/m33.0 pliDie B; Method D 624
Compression Set  9.1 %
@Temperature 70.0 °C,
Time 79200 sec
9.1 %
@Temperature 158 °F,
Time 22.0 hour
Solid
 12.7 %
@Temperature 70.0 °C,
Time 79200 sec
12.7 %
@Temperature 158 °F,
Time 22.0 hour
Plied
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -53.9 °C-65.0 °F
Shrinkage 8.4 %
@Temperature 100 °C,
Time 252000 sec
8.4 %
@Temperature 212 °F,
Time 70.0 hour
Volume, Distilled water aged
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRESL088 / 318298

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.