MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Proto Labs Aluminum AlSi10Mg - DMLS
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: AlSi10Mg is an aluminum master alloy often specified for casting or die casting parts. It has an excellent strength-to-weight ratio among aluminum alloys, but it has a lower elongation at break. It has good high-temperature characteristics, corrosion resistance, and fatigue resistance.

Due to its high strength-to-weight ratio, AlSi10Mg is a good choice among casting materials for automotive and aerospace applications, notably gearboxes, housings and brackets that are subject to high loading.

Information provided by Proto Labs.

Key Words: Direct Metal Laser Sintering; EN DIN 1706:2013; 3D Printing; Additive Manufacturing
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 47.2
Tensile Strength, Ultimate 37.7 ksi
Tensile Strength, Yield 31.9 ksi
@Strain 0.2 %
Elongation at Break 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum A360.0-F Die Casting Alloy
Aluminum 360.0-F Die Casting Alloy
3D Systems LaserForm® AlSi10Mg (A), AS-BUILT Aluminum Alloy Material
Aluminum A380.0-F Die Casting Alloy
Aluminum 6063-T5

NPROTO990 / 232384

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.