Overview: CALIBRE™ 303V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 303V-6 contains a mold release agent, a UV stabilizer additive, and is available in opaque white color only. Govt. and Industry Standards: - CSA (Canadian Standards Association)
- Underwriters Laboratory Inc. (UL)
Applications:- Electronic components
- Automotive
- Lighting
- Storage Media Housings
|