MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Bormed™ HF840MO Polypropylene Homopolymer for Medical Applications
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Bormed HF840MO is a polypropylene homopolymer intended for injection molding and is modified with an internal lubricant for products requiring a low surface friction (e.g. two-part syringes).

Bormed HF840MO is used in medical devices such as syringe barrels, needle covers, catheter connections, screw caps and closures, and medical valves.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm0.010 - 0.020 in/in
Melt Flow 19 g/10 min
@Load 2.16 kg,
Temperature 230 °C
19 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9393ISO 2039-2
Tensile Strength, Yield 29.5 MPa4280 psiAt 50 mm/min; ISO 527-2
Elongation at Yield 11 %11 %At 50 mm/min; ISO 527-2
Tensile Modulus 1.25 GPa181 ksiAt 1 mm/min; ISO 527-2
Charpy Impact, Notched 0.350 J/cm²1.67 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 260 °C410 - 500 °F
Mold Temperature 30.0 - 40.0 °C86.0 - 104 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Bormed™ RF830MO Polypropylene Copolymer for Healthcare Applications
Borealis Bormed™ HF855MO Polypropylene Homopolymer for Medical Applications
Borealis Bormed™ RF825MO Polypropylene Copolymer for Healthcare Applications
Total PPH 3620WZ Polypropylene, Injection Molding Grade
Borealis Bormed™ RG835MO Polypropylene Copolymer for Healthcare Applications

PBOREA074 / 27381

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.