Hostacom EP380X PC81 is an unfilled polypropylene copolymer, with high melt flow rate offering a good impact/stiffness balance. Product is available as a customized color matched, pellet form. This grade is delivered in PC81 color version. Applications: Interior Automotive ApplicationsInformation provided by LyondellBasell. |