MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Lupolen 5261Z Q456 POWDER High Density Polyethylene (HDPE), Pipe Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Lupolen 5261Z Q 456 POWDER is a high density polyethylene (HDPE) with very high melt viscosity for ram extrusion of peroxide cross-linked pipes (PEX-a). The product is supplied as a nominal 25 mesh (820 µm) powder. Applications: Drinking Water Pipe, Plumbing, Heating & Cooling, Under floor Heating

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.954 g/ccASTM D1505
Melt Flow 2.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D <= 71ASTM D 2240
 64
@Time 15.0 sec
ASTM D 2240
Tensile Strength at Break 40.5 MPaASTM D638
Tensile Strength, Yield 27.7 MPaASTM D638
Elongation at Break 900 %ASTM D 638
Elongation at Yield 8.1 %ASTM D 638
Tensile Modulus 1324 MPa1% secant; ASTM D638
2% Secant Modulus 1213 MPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 130 °CA1; ASTM D1525
 131 °CB1; ASTM D1525
 
Descriptive Properties
Processing MethodPipe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical SEETEC BF315 LDPE
Esenttia 03H83-AV Homopolymer Polypropylene
Ineos K38-20-138 Pipe Extrusion Grade Polyethylene
LyondellBasell Alathon® M6028 High Density Polyethylene
Formosa Plastics Formolene® HP4306 Pipe HDPE

PEQT8577 / 220212

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.