MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eneos DYNARON 4600P Styrene-(ethylene/butylene)-crystalline block copolymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Characteristics and applications: SEBC type provides polyethylene(PE) compounds with better transparency and flexibility without plasticizer due to fine dispersion of SEBC.

ENEOS has acquired the elastomer product lines from JSR Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 g/cc0.910 g/ccJIS K7210
Melt Flow 5.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.5 g/10 min
@Load 4.77 lb,
Temperature 446 °F
JIS K7210
 
Chemical PropertiesMetricEnglishComments
Styrene Content 20 %20 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7878JIS K7210
Tensile Strength 17.0 MPa2470 psiJIS K6251
Elongation at Break 680 %680 %JIS K6251
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D150
Dielectric Constant 2.45
@Frequency 1000 Hz
2.45
@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.0013
@Frequency 1000 Hz
0.0013
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -45.0 °C-49.0 °FJIS K7121

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJSRC8179 / 295495

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.