MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay FM® 94U Adhesive Film
Categories: Polymer; Film; Thermoset; Epoxy

Material Notes: Description: FM® 94 adhesive is a 220°F (104°C) service temperature, modified epoxy film adhesive designed for bonding metallic and composite structures. FM 94 adhesive offers a unique combination of high temperature performance, toughness and moisture resistance as demonstrated by its ability to bond to wet Nomex® honeycomb and retention of shear properties after pre- and post-bond humidity exposure. FM 94 adhesive is designed for applications demanding the best of both 220°F (104°C) service temperature and -67°F (-55°C) peel strength. For composite and metal bonding applications, FM 94 adhesive is formulated to exhibit superior elongation, toughness and shear strength properties. The controlled flow characteristics allow for its use in co-cured applications as well as bonding pre-cured structures. Also, FM 94 adhesive provides excellent electrical insulation between metal and graphite composites, reducing the potential for galvanic corrosion. FM 94 film adhesive is manufactured as a supported adhesive with both knit and mat carriers, or as an unsupported film. When supported with a knit carrier, optimal mechanical properties can be obtained. The random mat provides superior handling characteristics. With the mat carrier, FM 94 adhesive can be supplied in a one-side tacky (OST) version which helps reduce air entrapment when bonding large metal or composite parts.

Features & Benefits:

  • Demonstrates superior strength in bonding both metallic and composite structures
  • Provides structural performance from -67°F to 220°F (-55°C to 104°C)
  • Offers exceptional elongation and toughness
  • Higher service temperature version of FM® 73 film adhesive
Applications:
  • Bonding of metallic and composite structures
Note 1: Aluminum Substrate with BR® 6747-1 Adhesive Primer
Note 2: FM 94K 0.06 psf (293 gsm) Film Adhesive after Humidity, Salt Spray and Solvent Exposure, Aluminum Substrate with BR 6747-1 Adhesive Primer
Note 3: FM 94K 0.06 psf (293 gsm) Film Adhesive, Effect of Cure Cycle, Aluminum Substrates with BR 6747-1 Adhesive Prime
Note 4: FM 94K 0.06 psf (293 gsm) Film Adhesive with BR 6747-1 Adhesive Primer
Note 5: Effect of Humidity, Wet Nomex Bonding with FM 94M 0.06 psf (293 gsm) Film Adhesive, Immersed in water for 24 hours at 140°F (60°C) then bonded within 2 hours
Note 6: Composite Substrates Co-cure Data with FM 94M 0.06 psf (293 gsm) Film Adhesive
Note 7: Secondary Bonding of Epoxy/Graphite Substrates with FM 94M 0.06 psf (293 gsm) Film Adhesive

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.0 %
Storage Temperature -18.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 104 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
ColorGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay FM® 73U Epoxy Film Adhesive
Solvay FM® 94M Adhesive Film
Solvay FM® 94K Adhesive Film
Solvay FM® 94M OST Adhesive Film
Solvay FM® 99 Surfacing Film

PCYTED107 / 180409

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.