MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ EX7681T PC (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN EX7681T is a coextrusion product which is highly UV stabilised exhibiting low plate out and improved outdoor weathering of LEXAN sheet.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 63.0 MPa50 mm/min; ISO 527
Elongation at Break 120 %50 mm/min; ISO 527
Elongation at Yield 6.0 %50 mm/min; ISO 527
Tensile Modulus 2350 MPa1mm/min; ISO 527
Flexural Yield Strength 90.0 MPa2 mm/min; ISO 178
Flexural Modulus 2300 MPa2 mm/min; ISO 178
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 135 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Zone 1 240 - 280 °CProfile Extrusion
Zone 2 240 - 280 °CProfile Extrusion
Zone 3 220 - 240 °CProfile Extrusion
Zone 4 220 - 240 °CProfile Extrusion
Adapter Temperature 220 - 240 °CProfile Extrusion
Die Temperature 245 - 290 °CProfile Extrusion
Melt Temperature 220 - 250 °C
Drying Temperature 105 °CProfile Extrusion
Dry Time 2.00 - 3.00 hourProfile Extrusion
Precipitation Temperature 60.0 - 100 °CCalibrator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10451 / 243918

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.