MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm CYROLITE Med2 Acrylic-Based Multipolymer Compound
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Gamma Radiation Resistant, Molded

Material Notes: CYROLITE Med 2 compound is an impact-modified acrylic-based multipolymer for molding and extrusion of medical applications. Typical properties of CYROLITE compound are:
  • excellent chemical resistance to fats and oils
  • excellent bonding and welding capabilities
  • excellent bonding to PVC tubing
  • good impact strength
  • good light transmission
  • good resistance to EtO, gamma and E-beam sterilization
The special properties of CYROLITE Med 2 compound are:
  • superior resistance to lipids
  • superior resistance to alcohol
  • excellent ductility
Applications: Used for injection molding and extrusion of medical devices.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Bulk Density 0.650 g/ccASTM D1895
Water Absorption <= 0.38 %ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D951
Melt Flow 2.1 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 33ASTM D785
Tensile Strength at Break 5320 psiASTM D638
Elongation at Break 22 %ASTM D638
Elongation at Yield 3.9 %ASTM D638
Tensile Modulus 250 ksiASTM D638
Flexural Strength 8590 psiASTM D790
Flexural Modulus 240 ksiASTM D790
Izod Impact, Notched 2.20 ft-lb/in
@Diameter 6.35 mm
BAR; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 48.0 µin/in-°F
@Temperature 0.000 - 100 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 163 °F
@Thickness 6.35 mm
Annealed; ASTM D648
Vicat Softening Point 201 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 7.0 %ASTM D1003
Yellow Index -1.00 %ASTM E313
Transmission, Visible 85 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 425 - 480 °FCylinder Temp
Melt Temperature 420 - 480 °F
Mold Temperature 120 - 180 °F
Drying Temperature 160 °F
Dry Time 3 - 4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm Acrylite Plus® H-16 Acrylic Molding Compound
Evonik CYROLITE® Protect Acrylic-polycarbonate alloy
Röhm CYROLITE G20-HIFLO Acrylic-Based Multipolymer Compound
Borealis Daplen™ EE255AE Polypropylene TPO Compound
Röhm CYROLITE® Protect 2 Acrylic-polycarbonate alloy

PCYR00033 / 89037

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.