MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Rynite® RE19051 BK507 Polyethylene Terephthalate (PET)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass/Mineral Reinforced

Material Notes: 40% Glass/Mineral Reinforced Flame Retardant Polyethylene Terephthalate

Rynite RE19051 BK507 is a 40% glass and mineral reinforced flame retardant polyethylene terephthalate black resin.

Former DuPont product acquired by Celanese in 2022.

Key Words: PET-(MD+GF)40FR(17)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.73 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPaISO 527-1/-2
Elongation at Break 1.7 %ISO 527-1/-2
Tensile Modulus 11000 MPaISO 527-1/-2
Flexural Strength 170 MPaISO 178
Flexural Modulus 9700 MPaISO 178
Poissons Ratio 0.34
Charpy Impact, Notched 6.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+14 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+15 ohmIEC 62631-3-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 23.0 µm/m-°CISO 11359-1/-2
 14.0 µm/m-°C
@Temperature 55.0 - 160 °C
ISO 11359-1/-2
 23.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 78.0 µm/m-°CISO 11359-1/-2
 61.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
 110 µm/m-°C
@Temperature 55.0 - 160 °C
ISO 11359-1/-2
Melting Point 247 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 214 °CISO 75-1/-2
Flammability, UL94 V-0
@Thickness 0.810 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 5VA
@Thickness 1.50 mm
IEC 60695-11-20
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °COptimum, Injection
 270 - 290 °CRange, Injection
Mold Temperature 110 °COptimum, Injection
 100 - 120 °CInjection
Ejection Temperature 170 °CInjection
Drying Temperature 120 °CInjection
Dry Time 4.00 - 6.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.020 %Injection
Hold Pressure >= 80.0 MPaInjection
 
Descriptive Properties
AdditivesFlame retardant
Back pressureAs low as possible
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PET-(GF+MD)40FR(16)<ISO 11469
PolymerPET-(GF+MD)40 FR(17)
Processing Hold Pressure Time (s/mm)4Injection
Regional AvailabilityAsia Pacific
Resin IdentificationPET-(GF+MD)40FR(16)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Rynite® FR530L BK507 Polyethylene Terephthalate (PET)
Celanese Rynite® 408 NC010 PET
Celanese Rynite® RE15022 NC010 Polyethylene Terephthalate (PET)
Dow LIGHTER™ S93 Polyethylene Terephthalate (PET) Resin
Dow LIGHTER™ S98 Polyethylene Terephthalate (PET) Resin

PDSY5285 / 161112

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.