MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
IDI Composites E-203 Thermoset Polyester, Sheet
Categories: Polymer; Thermoset; Composite SMC; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: ELECTRICAL - U.L. recognized (E53587). Designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resistance. Designed to meet critical impulse and corona specifications.

Data provided by IDI Composites.

Key Words: SMC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 - 1.90 g/ccASTM D792
Water Absorption 0.10 %in 24 hours; ASTM D570
Linear Mold Shrinkage 0.00 - 0.0020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 30 - 50ASTM D2583
Tensile Strength, Ultimate 55.0 MPaASTM D638
Flexural Strength 124 MPaASTM D790
Flexural Modulus 10.0 GPaASTM D790
Compressive Strength 166 MPaASTM D695
Izod Impact, Notched 4.27 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 16.0 kV/mmASTM D149
Arc Resistance >= 180 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °CASTM D648
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0
@Thickness 1.20 mm
 V-0
@Thickness 1.50 mm
 
Descriptive Properties
Bulk Factor App.1ASTM D1895

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass
A. Schulman Premi-Glas® 1200-30 Polyester SMC
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP
Quantum Composites QC-7810 55% Glass Fiber Polyester SMC
A. Schulman Premi-Glas® 1200H-20 Polyester SMC

PPTSBI / 58289

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.