MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Struktol CARSTAB® DLTDP Thioester Antioxidant
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Thioester synergist that is particularly effective as a long term heat aging stabilizer when used in conjunction with primary antioxidants.

  1. CARSTAB DLTDP is especially recommended to protect high density polyethylene and ABS from oxidation in high temperature applications.
  2. CARSTAB DLTDP is also very effective in polypropylene and other polymers.
  3. For applications requiring superior heat stability, a combination of a hindered phenolic antioxidant and CARSTAB DLTDP should be used. It has been found that a combination of three parts of CARSTAB DLTDP is one part of hindered phenolic antioxidant often provides optimum performance. Typical use levels are 0.15% of CARSTAB DLTDP and 0.05% of phenolic antioxidant. It is recommended that specific end use formulations be optimized with regard to thioester synergist ratio and use level.

FDA Status: 175.3

Key Words: C30H58O4S
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.896 g/cc
@Temperature 80.0 °C
0.896 g/cc
@Temperature 176 °F
Additive Loading >= 0.15 %>= 0.15 %Typical
Molecular Weight 514 g/mol514 g/mol
 
Chemical PropertiesMetricEnglishComments
Acid Value 0.500.50
 
Thermal PropertiesMetricEnglishComments
Melting Point 40.0 °C104 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 95 %95 %440 mu
 
Descriptive Properties
AppearanceWhite Crystalline Flakes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTRUK36 / 69264

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.