CF 10% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent characteristics of polycarbonate resin Applications: Mechanical, electric and electronic components that need abrasion and friction resistance.Information provided by Teijin Chemicals Ltd. |