MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Borcom™ WG140AI Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Borcom™ WG140AI is a polypropylene microcomposite intended for injection molding. This material has an excellent balance between impact strength and stiffness, high melt flow rate and gives a good surface quality. Applications: Borcom™ WG140AI has been developed especially for applications like: washing machine parts, control panels washing applications, dishwashers components, climate control housings, and air ducts.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/ccISO 1183
Linear Mold Shrinkage 0.012 cm/cmmold average, Borealis Method
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 37.0 MPa50mm/min; ISO 527-2
Elongation at Yield 5.0 %ISO 527-2
Tensile Modulus 2600 MPa1mm/min; ISO 527-2
Charpy Impact Unnotched 25.0 kJ/m²
@Temperature -20.0 °C
ISO 179/1eU
 70.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.50 kJ/m²
@Temperature -20.0 °C
ISO 179/1eA
 3.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 125 °C
@Thickness 2.00 mm
EN 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 64.0 °CISO 75-2
 120 °CISO 75-2
Vicat Softening Point 94.0 °C
@Load 5.10 kg
ISO 527-2
 155 °C
@Load 1.02 kg
ISO 527-2
Flammability, UL94 HB
@Thickness 2.00 mm
Flame Spread 23 mm/min
@Thickness 3.00 mm
FMVSS 302; DIN 75200
Glow Wire Ignition Temperature 800 °C
@Thickness 2.00 mm
EN 60695-2-13
Glow Wire Flammability Index 825 °C
@Thickness 2.00 mm
EN 60695-2-12
 
Optical PropertiesOriginal ValueComments
Gloss 50 %2mm plaque, 20° of arc; DIN 67530
 
Processing PropertiesOriginal ValueComments
Feed Temperature 40.0 - 80.0 °C
Melt Temperature 220 - 260 °Cmass temperature
Mold Temperature 30.0 - 50.0 °C
Injection Velocity 100 - 200 mm/sec
Hold Pressure 30.0 - 60.0 MPa
 
Descriptive Properties
Back Pressurelow to medium
Emission (µgC/g)35VDA 277
Fogging (mg)1.4100°C, 16h, DIN 75201
Screw Speedlow to medium

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Addiplast Addilene H 530 N30 Polypropylene Homopolymer
LyondellBasell Adstif HA 840R Polypropylene
Amco PRIMATOP PP HOMO 350NA Injection Molding Polypropylene
Amco PRIMATOP PP HOMO 120NA-HF Multi-Purpose Polypropylene
Borealis Daploy™ WB140HMS Polypropylene

PBOREA368 / 108628

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.