MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® F593 Epoxy Resin, T2G190 Carbon Tape
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Hexcel designation: T2GXXX-12"-F593; Fiber: Amoco T-300/12k

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Filler Content 50.0 - 55.0 %Laminate Fiber Volume
Volatiles 1.0 - 4.0 %Prepreg
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3.372 MPa
@Temperature 93.0 °C
Sandwich Flatwise Tension, Dry
 5.192 MPa
@Temperature 24.0 °C
Sandwich Flatwise Tension, Dry
 1269 MPa
@Temperature -54.0 °C
Dry
 1331 MPa
@Temperature 24.0 °C
Dry
 1427 MPa
@Temperature 71.0 °C
Dry
 1751 MPa
@Temperature 93.0 °C
Dry
Tensile Modulus 120 GPa
@Temperature 24.0 °C
Dry
 121.4 GPa
@Temperature 71.0 °C
Dry
 123.4 GPa
@Temperature -54.0 °C
Dry
 126.2 GPa
@Temperature 93.0 °C
Dry
Compressive Yield Strength 183 MPa
@Temperature 24.0 °C
Compression After Impact, Dry
 1234 MPa
@Temperature 71.0 °C
Wet
 1455 MPa
@Temperature 93.0 °C
Dry
 1538 MPa
@Temperature 71.0 °C
Dry
 1655 MPa
@Temperature 24.0 °C
Dry
 1786 MPa
@Temperature -59.0 °C
Dry
Compressive Modulus 108.3 GPa
@Temperature -59.0 °C
Dry
 113.8 GPa
@Temperature 93.0 °C
Dry
 114.5 GPa
@Temperature 24.0 °C
Dry
 115.1 GPa
@Temperature 71.0 °C
Dry
 
Descriptive Properties
Cured Thickness per Ply (cm)0.02-0.021Laminate
Dry Resin Content (%)36-40Prepreg
Flow (%)13-25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® F593 Epoxy Resin, T2G095 Carbon Tape
Hexcel® HexPly® F593 Epoxy Resin, T2G145 Carbon Tape
Hexcel® HexPly® F593 Epoxy Resin, W3G282 Carbon Fabric
Hexcel® HexPly® F593 Epoxy Resin
Hexcel® HexPly® F593 Epoxy Resin, F3T584 Carbon Fabric

PHEXC151 / 98621

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.