MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polytek 74-30 Clear Flexible, High-Strength, Polyurethane Mold Rubbers
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Poly 74-Series Liquid Rubbers consist of two parts (A and B), which, after mixing, cure at room temperature to flexible, high-strength, mold rubbers. Poly 74-Series Rubbers make durable, easy-releasing molds for casting plasters and waxes without release agents. When Poly 74-Series molds are properly prepared, they are also excellent for casting concrete and various resins, such as epoxy, polyester, polyurethane and acrylic.

Product Line Features:

  • Make durable, long-lasting molds owing to strength and elongation properties of cured rubber
  • Pourable liquid rubbers that cure to soft to mid-range hardnesses
  • Easily thickened for brush-on applications
  • No release agents needed when casting many plasters, waxes and concretes
  • Low-viscosity liquid rubbers capture detail from intricate masters

Information provided by Polytek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/cc
Viscosity 2000 cP2000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030
Tensile Strength 1.94 MPa281 psi
Elongation at Break 507 %507 %
Tear Strength 10.9 kN/m62.0 pliDie C Tear
 
Processing PropertiesMetricEnglishComments
Cure Time 25.0 - 30.0 min0.417 - 0.500 hourPour Time
 960 min16.0 hourDemold Time
 
Descriptive Properties
Cured ColorTransparent Amber
Mix Ratio By Weight1A:1B
Specific Volume27.5 in3/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTK5033 / 251025

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.