Notes: Medalist MD-84300 series are high performance thermoplastic elastomer designed specifically for extrusion and injection molded electrical applications in the medical and healthcare industry. The Medalist MD-84300 series are a better alternative to traditional TPVs used in such applications. Medalist MD-84388 is a higher hardness, low density grade with good electrical properties and can be sterilized by autoclave, ETO, or gamma radiation. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Autoclave Sterilizable; Electrically Insulating; Ethylene Oxide Sterilizable; Good Color Stability; Good Colorability; Good Sterilizability; Halogen Free; High Tensile Strength; Low Density; Medium Flow; Radiation Sterilizable; Slip Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment; Wire & Cable Applications RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion; Injection Molding Preliminary data. Information provided by Teknor Apex |