MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Röhm ACRYLITE® Resist AG 100 Acrylic polymer
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Extruded

Material Notes: ACRYLITE® Resist AG 100 is an amorphous thermoplastic molding compound, based on impact modified polymethyl methacrylate (PMMA).

ACRYLITE® molding compounds have the following typical properties:

  • high weather resistance
  • excellent transmission and clarity
  • brilliant appearance
  • low weight
  • 100% recyclable
  • pleasant feel and sound of molded parts
ACRYLITE® Resist AG 100 is characterized by the following additional properties:
  • highest breaking strength and impact strength
  • improved resistance to stress cracking
  • balanced property profile
  • clear reduction of reversible haze at very high and low temperatures
  • increased heat deflection temperature under load
  • AMECA listing, CAMPUS and moldflow data available
Application: ACRYLITE® Resist AG 100 has a balanced property profile and is used for extruding and coextruding sheets and profiles as well as for injection molding.

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccISO 1183
Water Absorption 0.50 %50% Humidity; ISO 62
 1.5 %saturation, in Water; ISO 62
Melt Flow 1.1 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 55.0 MPa50 mm/min; ISO 527
Elongation at Break 45 %Nominal; ISO 527
Elongation at Yield 5.0 %50 mm/min; ISO 527
Tensile Modulus 2.20 GPa1 mm/min; ISO 527
Charpy Impact Unnotched 120 kJ/m²ISO 179/1eU
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 105 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 100 °CISO 75
Vicat Softening Point 105 °CB / 50; ISO 306
Glass Transition Temp, Tg 112 °CISO 11357
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49
@Wavelength 589 nm
ISO 489
Haze 0.70 %ASTM D1003
Transmission, Visible >= 91 %ISO 13468-2
 
Processing PropertiesOriginal ValueComments
Die Temperature 240 °CExtrusion
Melt Temperature 235 - 270 °C
Mold Temperature 60.0 - 80.0 °CInjection Molding
Drying Temperature 70.0 - 80.0 °CPredrying
Dry Time 3.00 - 4.00 hourPredrying, Desiccant-Type Drier

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROHM9331 / 319948

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.