MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polykemi AB POLYasa 3010F Extra High Flow ASA
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes:

Information provided by Polykemi AB

Key Words: ASA
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inISO 2577
Melt Index of Compound 30 g/10 min
@Load 10.0 kg,
Temperature 220 °C
30 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break <= 42.0 MPa<= 6090 psiISO/R527
Elongation at Yield 6.0 %6.0 %ISO/R527
Flexural Strength <= 85.0 MPa<= 12300 psiISO 178
Flexural Modulus 2.60 GPa
@Temperature 23.0 °C
377 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched  0.500 J/cm²
@Temperature -20.0 °C
2.38 ft-lb/in²
@Temperature -4.00 °F
ISO 179
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C201 °F120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °F120°C/h; ISO 75/1
Vicat Softening Point  92.0 °C
@Load 5.001 kg
198 °F
@Load 11.03 lb
50°C/h; ISO 306
 101 °C
@Load 1.00 kg
214 °F
@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Glow Wire Test 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
IEC 695-2-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 230 °C374 - 446 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2 - 4 hour2 - 4 hourin circulation dryer
 2 - 4 hour2 - 4 hourin fresh-air dryer
 2 - 4 hour2 - 4 hourin desiccant air dryer
Injection Pressure 90.0 - 150 MPa13100 - 21800 psi
Back Pressure 1.00 - 1.50 MPa145 - 218 psi
 
Descriptive Properties
Holding Pressure20-40% of injection pressure
Injection SpeedHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® WR-9100 ASA, Unreinforced
Lotte Advanced Materials Starex® WR-9310 ASA, Unreinforced Heat Resistant
Omni Plastics OmniTech™ ASA 220 ASA
Lotte Advanced Materials Starex® WR-9370 ASA, Unreinforced Heat Resistant
Lotte Advanced Materials Starex® WR-9300HF ASA, Unreinforced Heat Resistant

PPOLYK005 / 122730

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.