MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Reynolds Matrix Dryve™ All-powder polymer modified gypsum system
Categories: Other Engineering Material

Material Notes: Product Overview: Matrix Dryve™ is a versatile all-powder polymer modified gypsum system that has superior physical and performance properties compared to regular gypsum products. It is an “all-powder” alternative to our original Matrix™ NEO powder/liquid system. The mix ratio of Dryve™ is 3 parts Dryve™ powder to 1 part water by volume (100 parts Dryve™ powder to 27 parts water by weight). Dryve™ is easy to use and can be cast solid, slush cast, rotationally cast, laid up by hand with chopped glass fiber or sprayed. Dryve™ can be thickened using Matrix™ Thickener, accelerated using Matrix™ Accelerator and slowed using Matrix™ Retarder. Fully cured pieces are strong, water-resistant and can be painted, sanded, machined and more. Dryve™ certifies to the highest flame rating (UL-94V-O / ASTM E-84 - Class A), making it suitable for public space applications including creating themed environment elements, architectural elements, sculpture and more. Versatility – Dryve™ can take you in many creative directions by allowing you to make a variety of finish effects including different colors, metallics, glitters, stone and more (see Creating Finished Effects section).

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.584 g/cc1.584 g/cc
Water Absorption <= 0.50 %<= 0.50 %after 24 hour water soak
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 22.8 - 37.9 MPa3300 - 5500 psi
Flexural Strength 51.7 - 67.6 MPa7500 - 9800 psi
Compressive Strength 44.8 - 65.5 MPa6500 - 9500 psi
Tensile Impact Strength 367 kJ/m²175 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 90.0 min1.50 hourDrill Mixed
Pot Life 20.0 min20.0 minDrill Mixed
 
Descriptive Properties
ColorWhite
Freeze/Thaw Resistance300 cycles
Mix Ratio100:27Powder: Water by Weight
 3:1Powder: Water by Volume
Specific Volume17.45[in3/lb]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN317 / 297018

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.