MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
WNiFe Class 3 Tungsten Alloy
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: W-3.5Ni-1.5Fe

Vendors: Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 17.992 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 27 - 34
Tensile Strength, Ultimate 827 MPa
Tensile Strength, Yield 621 MPa
@Strain 0.2 %
Elongation at Break 7.0 %
Modulus of Elasticity 345 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00001332 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.60 µm/m-°C
Thermal Conductivity 26.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe 1.5 %
Nickel, Ni 3.5 %
Tungsten, W 95 %As balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
WNiFe Class 1 Tungsten Alloy
WNiFe Class 2 Tungsten Alloy
WNiCu Class 1 Tungsten Alloy
WNiCu Class 3 Tungsten Alloy
Tungsten Alloy A90

MW906 / 100374

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.