MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polyplastic Compounds Technoter® A-GF 30-FR PBT, 30% Glass Fiber Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: A 30% glass fiber, fire retardant polybutylene terephthalate. Designed for injection molding and extrusion of various items and parts for construction, electrical tools, machine engineering, household appliances, transportation, camping equipment etc.

Information provided by Polyplastic Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.011 cm/cmISO 294-4
Melt Flow 27 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 135 MPaISO 527-1
Elongation at Break 3.0 %ISO 527-1
Flexural Strength 214 MPaat maximum load; ISO 178
Flexural Modulus 9500 MPaISO 178
Charpy Impact Unnotched 40.0 kJ/m²
@Temperature -40.0 °C
ISO 179-1
 44.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -40.0 °C
ISO 179-1
 9.00 kJ/m²
@Temperature 23.0 °C
ISO 179-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Dielectric Strength 26.0 kV/mmIEC 60243
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°CISO 11359-2
Melting Point 222 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 210 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °C
Mold Temperature 90.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLPLC149 / 307221

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.