MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Northstar Polymers MPP-W43C Polyurethane Gel
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: MPP-W43C is a polyurethane gel formulation specifically designed for padding and cushioning applications that require Shore Durometer OOO scale hardness materials. With this material, a user can obtain good rebound characteristics and gradual compression deflection rates at the Shore OOO hardness range. The material does not contain any plasticizer, which is known to leach out to have adverse effect to the plastic film encapsulation materials used in conjunction with gel materials.

This formula uses the same part-B (PNA-157) as standard Shore OO polyurethane gel. This allows you to make variety products with fewer raw material inventories. The applications for this material include cushioning and padding parts for medical/semi-medical application, fiber optic cable encapsulation, novelty products, and many more.

This polyurethane gel material is formulated in such a way that the user can control/choose the hardness/deflection properties of the product.

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 72.0 - 86.0 °FPrepolymer Temperature
 72.0 - 86.0 °FCuring Agent Temperature
Mold Temperature 72.0 - 86.0 °F
Cure Time 2.00 - 5.00 hour
@Temperature 25.0 °C
De-mold Time
 24.0 - 48.0 hour
@Temperature 25.0 °C
Complete Cure Cycle
Pot Life 5.00 min
 
Descriptive Properties
Curing AgentPNA-157
PrepolymerMPC-070
Weight Ratio1:4.009Prepolymer to Curing Agent Ratio, Shore Hardness OOO 65
 1:4.556Prepolymer to Curing Agent Ratio, Shore Hardness OOO 55
 1:5.103Prepolymer to Curing Agent Ratio, Shore Hardness OOO 40
 1:5.285Prepolymer to Curing Agent Ratio, Shore Hardness OOO 35
 1:5.467Prepolymer to Curing Agent Ratio, Shore Hardness OOO 30
 1:5.65Prepolymer to Curing Agent Ratio, Shore Hardness OOO 25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets
Northstar Polymers MPP-V37A Polyurethane Gel Elastomer
Northstar Polymers MCP-V40A Polyurethane Gel
Northstar Polymers MPC-W44A Polyurethane Gel
AorTech Biomaterials ECSil™ 70A Biomedical Carbonate Silicone Pellets

PNORTH858 / 162574

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.