MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nitriflex SB-4022 Styrene Butadiene Copolymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes:

Applications: Powdered rubber. Enables a lower mixing time and better homogenization, presenting a reduced generation of residues. Recommended for shoe soles, adhesives and seals, injected and molded artifacts.

Information provided by Dax Resinas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 0.00 - 0.75 %Method B-003; ASTM D5668
Particle Size <= 1000 µm99-100%; ASTM D1921
Mooney Viscosity 46 - 58
@Temperature 100 °C
MML1+4, Method B-002; ASTM D1646
 
Chemical PropertiesOriginal ValueComments
Styrene Content 22.5 - 24.5 %ASTM D5775
 
Descriptive Properties
CaCO3 Partitioning Agent Content %10 to 14Method B-035

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dynasol Solprene® 303 Random-Block Copolymer
Nitriflex SB-1015 Styrene Butadiene Copolymer
Nitriflex SB-1013G Styrene Butadiene Copolymer
Dynasol Calprene® 1015 Styrene-Butadiene Rubber SBR Diblock Copolymer

PDAX058 / 29483

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.