MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Daikin OPTOOL UD120 Coating Agent
Categories: Other Engineering Material

Material Notes: OPTOOL UD120 is an antifouling coating agent with excellent weather resistance. UD120 shows excellent performance in stain resistance, chemical resistance and surface slippery under UV exposure condition.

Introduction: Excellent water and oil repellency; Good anti finger print property; Maintain excellent water and oil repellency with superb UV resistant; Super thin film coating and no impact for optical properties; Reduce sliding contact angle; Non-stick and low surface energy; Cures with Glass, SiO2 and AR surface in the room temperature; Excellent acid / base resistant

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Surface Tension 13.0 dynes/cm
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction 0.0700LabthinkFPT-1, Load: 200g, Speed: 200mm/min, friction material: paper
 
Optical PropertiesOriginal ValueComments
Haze 0.250 %
 
Descriptive Properties
Contact angle115°water
Sliding anglen-hexadecane
 water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDAIK9746 / 327186

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.