System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
422 Stainless Steel 315°C (600°F) temper
Categories:
Metal
;
Ferrous Metal
;
Stainless Steel
;
T 400 Series Stainless Steel
Material Notes:
austenitized at 1040°C for 1 hour, oil quench, temper for 2 hours
Key Words:
UNS S42200, AMS 5655, ASTM A565, SAE J467, DIN 1.4935, JIS SUH 616
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
7.80
g/cc
Mechanical Properties
Original Value
Comments
Tensile Strength, Ultimate
1580
MPa
Tensile Strength, Yield
1000
MPa
@Strain 0.2 %
Elongation at Break
16 %
in 36 mm
Tensile Modulus
199.2
GPa
141.4
GPa
@Temperature 595 °C
166.6
GPa
@Temperature 425 °C
189.6
GPa
@Temperature 260 °C
Poissons Ratio
0.20
Calculated
Shear Modulus
62.0
GPa
@Temperature 593 °C
72.4
GPa
@Temperature 427 °C
79.3
GPa
@Temperature 260 °C
82.7
GPa
@Temperature 23.9 °C
Electrical Properties
Original Value
Comments
Electrical Resistivity
0.0000610
ohm-cm
Thermal Properties
Original Value
Comments
CTE, linear
11.2
µm/m-°C
@Temperature 0.000 - 100 °C
11.3
µm/m-°C
@Temperature 0.000 - 315 °C
11.9
µm/m-°C
@Temperature 0.000 - 540 °C
12.1
µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity
0.460
J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity
23.9
W/m-K
@Temperature 100 °C
27.3
W/m-K
@Temperature 500 °C
Melting Point
1470
-
1480
°C
Solidus
1470
°C
Liquidus
1480
°C
Component Elements Properties
Original Value
Comments
Carbon, C
0.20 - 0.25 %
Chromium, Cr
12 %
Iron, Fe
84 %
Manganese, Mn
<= 1.0 %
Molybdenum, Mo
1.0 %
Nickel, Ni
0.75 %
Phosphorus, P
<= 0.025 %
Silicon, Si
<= 0.75 %
Sulfur, S
<= 0.025 %
Tungsten, W
1.0 %
Vanadium, V
0.23 %
References
for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
422 Stainless Steel, 455°C temper, short time elevated temperature test
440A Martensitic Stainless Steel (UNS S44002)
440C Martensitic Stainless Steel (UNS S44004)
410 Stainless Steel
420 Stainless Steel
MQ422AH / 13091
Free Trade Publications, Click Here!
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.